Every time PA66 prices move, this question returns. The answer is not yes or no — it is under which conditions.
| Property | PA6 + 0.3–0.4% | Verdict |
|---|---|---|
| Tensile strength | 185 MPa | Meets or exceeds |
| Flexural modulus | 9100 MPa | Meets or exceeds |
| Notched Izod impact | 19.7 kJ/m² | Meets or exceeds |
| Heat distortion temperature | Below PA66 | Not met |
Third-party test report. HDT is an intrinsic difference between PA6 and PA66 and cannot be fully closed by additives.
A major nylon producer built a PA6 reinforcing masterbatch on our additive. Added at 20% to PA6, it reaches tensile strength above 70 MPa and notched impact above 6.0 kJ/m², injection mouldable directly as a masterbatch. It has partially replaced PA66 in cable-tie compounds.
Intra-molecular lubrication improves fibre wet-out. In 35% glass-fibre PP, modulus and impact both rise while flow improves and processing temperature falls. The same mechanism applies in glass-fibre PA.
At 1.5–3.0% of our targeted antimicrobial masterbatch, PA fibre fabrics and nonwoven reach Grade 0 mildew and fungal resistance, with no effect on spinning.
Please provide PA6 viscosity grade, glass-fibre content, moulding temperature and the PA66 grade you are benchmarking.
Request a sampleTell us your resin grade, processing temperature, part thickness and the property you need to improve. We recommend a grade and dosage, ship 1–5 kg, and follow up with comparative data.
Or call Mr. Luo +86 135 5407 7117 +86 130 0101 5295