This series does one thing: brings recycled material back to virgin performance, and lets virgin material go further. It replaces POE and LLDPE, not nucleating agents.

It replaces the impact modifier, not the nucleator

The standard industry answer to poor recyclate toughness is 10–20% POE or LLDPE in the formulation. The cost is explicit: modulus drops, cost rises, the melt thickens and processing gets harder.

Tinapec™ inverts the approach: 1.5–3% of a functional masterbatch raises stiffness, toughness and flow at the same time — because the mechanism is nucleation and lubrication, not dilution.

In grade-3 recycled PP, 3% E2801 lifts notched Izod impact from 16.05 to 57.53 kJ/m² (+258%) while flexural modulus rises 6%. That combination exceeds virgin K8003.

Grades

GradePositioningTypical use
E2415Main recyclate toughenerVirgin + grade-5 recyclate, premium + low-grade blends
E2415XEconomy version of E2415Cost-sensitive formulations with slightly lower targets
E2801POE8150 replacementGrade-3 recyclate, stiffening and toughening together
E2430R1POE6202 replacementGrade-3 recyclate, balancing modulus and impact

E2005 and E2220 are available for in-reactor addition and automotive compounding. Please confirm grade selection with us.

Data

A different formulation for each recyclate grade

PP recyclate is commonly classified in six grades by notched impact and elongation at break. One grade cannot serve all of them.

Base formulationAs receivedAdditionResult
80% K8003 + 20% grade-5 recyclate922 MPa / 18.6 kJ/m²+1.5% E2415Modulus +5%, impact 52.0 (+180%)
80% grade-1 + 20% grade-5829 MPa / 18.3 kJ/m²+2.0% E2415Modulus +5%, impact 42.8 (+134%)
Grade-3 recyclate854 MPa / 16.05 kJ/m²+3% E2801Modulus +6%, impact 57.53 (+258%)
Grade-3 recyclate854 MPa / 16.05 kJ/m²+3% E2430R1860 MPa, impact 54.70 (+241%)
Grade-3 recyclate (control)854 MPa / 16.05 kJ/m²+3% POE8150836 MPa, impact 54.57

The last row is the conventional modifier. Impact rises, modulus falls. With E2801 impact is higher and modulus rises.

Test it before you price it

Tell us your resin grade, processing temperature, part thickness and the property you need to improve. We recommend a grade and dosage, ship 1–5 kg, and follow up with comparative data.

Or call Mr. Luo +86 135 5407 7117 +86 130 0101 5295