Home/Applications/Woven bags
01 / Woven bags & FIBC

Woven bags and FIBC

Thin margins, high electricity share, extreme sensitivity to grammage. Here, "lower processing temperature" and "higher strength at equal weight" translate directly into money.

Three improvements you can book

1. Higher strength at equal weight — or lower weight at equal strength

With higher tape tensile and stiffness, grammage can come down at the same load rating. In FIBC, grammage is cost.

2. Lower tape extrusion temperature

Intra-molecular lubrication reduces melt viscosity, so barrel zone temperatures can be reduced. In a plant running tape lines 24 hours a day, this line item often exceeds the masterbatch cost.

3. Higher recyclate content

Woven goods are one of the largest recyclate users. As recyclate content rises, tape strength falls and break rate climbs. At 1.5–3% Tinapec™ the same recyclate ratio holds its original strength — or the same strength can be reached at a higher recyclate ratio.

One caveat

Woven formulations use large amounts of calcium carbonate filler. At high filler loading the lubrication effect is more pronounced, so the masterbatch loading needs to be re-confirmed rather than defaulted to 1.5%. Please tell us your filler ratio.

Test it before you price it

Tell us your resin grade, processing temperature, part thickness and the property you need to improve. We recommend a grade and dosage, ship 1–5 kg, and follow up with comparative data.

Or call Mr. Luo +86 135 5407 7117 +86 130 0101 5295