Home/Insights/Grade 0 mildew
ANTIMICROBIAL

How Grade 0 mildew resistance is achieved

Many assume a poor rating means too little additive. In practice, adding more often makes it worse.

What Grade 0 means

Mildew testing grades samples by fungal growth on the surface. Grade 0 means no hyphal growth visible even under microscopy — the highest rating. Grade 1 means invisible to the eye but visible under magnification, and so on.

To reach Grade 0, a mixed mould spore population must be suppressed continuously for the full test period, typically 28 days. That demands persistence, not toxicity.

Why "add more" does not work

Three reasons:

  • Heat — most organic biocides begin decomposing between 200 and 230 °C, exactly the processing window, and spinning is hotter. Adding more means more decomposition, and the residue may cause odour and VOC.
  • Dispersion — if the biocide agglomerates, local concentration is excessive (creating defects) while other regions are under-dosed. Total loading looks adequate; effective surface area is not.
  • Migration — some biocides migrate to the surface and are lost, working early and failing later. Over a 28-day test the grade drops.

Our three responses

1. Stability above 250 °C

The decomposition onset is above 250 °C, covering conventional processing for PP, PE, PA and PVC and most spinning processes. Combined with no odour, low VOC and no toxicity, that is the precondition for fibre and food-contact work.

2. Dispersion completed during manufacture

Rather than dispersing inside the polymer, we form a micro-nano dispersion during masterbatch production. What enters the melt is already separated and does not re-agglomerate.

3. Controlled release from a composite carrier

The active is held in a composite carrier and released progressively rather than exposed all at once. That avoids local over-concentration and extends the effective period.

Measured result

At 1.5–3.0% in PA6 and PA66, PA fibre fabrics and nonwoven reach Grade 0 mildew and fungal resistance with no effect on spinning, and comply with FDA food-contact requirements.

To be precise: complies with requirements, not "FDA certified", which is a registration procedure for specific products and facilities.

Practical notes

  • Fibre customers must state spinning temperature; above 280 °C requires dedicated thermal validation
  • For white and light-coloured parts, check colour shift by trial first
  • Mildew resistance is a surface phenomenon; surface roughness and coatings affect real performance
  • For continuous immersion or high humidity, validate under actual conditions rather than relying on the standard test alone

Test it before you price it

Tell us your resin grade, processing temperature, part thickness and the property you need to improve. We recommend a grade and dosage, ship 1–5 kg, and follow up with comparative data.

Or call Mr. Luo +86 135 5407 7117 +86 130 0101 5295