Home/Insights/UVB 1200 h
DURABILITY

What 1200 hours of UVB actually tells you

The industry circulates conversions such as "1000 hours equals five years outdoors". Here is why we do not use them.

First, the conclusion

Accelerated hours cannot be converted directly into service years. The same 1200 hours corresponds to very different service life in Hainan, Xinjiang, the Middle East or Scandinavia. Any fixed conversion factor is unsound.

So we report two things only: the test conditions (lamp type, hours, cycle) and the result (retention, colour shift). The conversion is left to the customer, who knows the climate.

Three common accelerated tests

TypeSourceCharacterTypical use
UVB-313Short-wave fluorescentAggressive; includes short wavelengths absent from sunlight, may cause non-natural degradationRapid screening, QC
UVA-340Long-wave fluorescentSpectrum near 340 nm approximates daylight; better correlationFormulation comparison, life estimation
Xenon arcXenon lampFull spectrum, closest to daylight; expensive and slowFormal certification, external reports

The point: UVB is fast and aggressive — good for ranking options, poor for predicting years. Service-life claims based only on UVB data often fail outdoors.

Four variables that break the conversion

  • Irradiance — annual total varies widely; plateaus and tropics far exceed temperate zones
  • Temperature — photo-oxidation accelerates markedly with temperature
  • Humidity and condensation — for some systems, hydrolysis and condensation cycles do more damage than light alone
  • Other factors — coastal salt spray, industrial sulphur compounds, pesticide contact, mechanical stress

These carry completely different weights by application. Agricultural film faces pesticides and high irradiance; pallets face load and thermal cycling; outdoor toys face repeated impact and sun. No single factor covers them.

So what is the 1200-hour figure good for?

A great deal, used correctly:

  • Comparison — under identical conditions, 89% versus 8% is real and repeatable, and shows one formulation is clearly better
  • Screening — eliminate weak options quickly without waiting years outdoors
  • Trend — the shape of the curve matters more than a single value: gradual decline or cliff-edge failure

The correct approach

  1. Accelerated testing for direction
    Rank formulations and eliminate failures.
  2. Outdoor exposure in the target climate
    Actual coupons, actual conditions. The Group operates an outdoor exposure site in Guangzhou that supports this.
  3. Establish a correlation
    Relate accelerated and natural data for the same formulation. That relation is valid only for that system and that climate.
  4. Keep a safety margin
    Design for the worst case, not the average.

Reading our data

After 1200 h UVB, Tinasup™ E2625 retains 89% gloss against 8% for the LLDPE control; after 2400 h UVA, elongation retention is 95% against 23%.

What these show is that the durability capability of the two formulations differs by an order of magnitude. How many years your pallet lasts in Guangdong or Inner Mongolia depends on your conditions — which is why we ask about service environment early.

Test it before you price it

Tell us your resin grade, processing temperature, part thickness and the property you need to improve. We recommend a grade and dosage, ship 1–5 kg, and follow up with comparative data.

Or call Mr. Luo +86 135 5407 7117 +86 130 0101 5295