From 128 seconds to 74: where the electricity goes

Buyers usually price the masterbatch and ignore the cycle. This note is about the cycle.

Where the time in a cycle goes

An injection cycle has four phases: filling, holding, cooling, ejection. For thick parts such as pallets, cooling accounts for 60–70% of the cycle. The main lever is cooling, not injection speed.

Cooling time depends on two things: how much heat must be removed to reach ejection temperature, and when the material becomes stiff enough to eject — that is, when crystallisation has progressed far enough.

A nucleator acts on the second: it starts crystallisation at a higher temperature and completes it faster, so the part can be ejected sooner. That is why 2% of a nucleating masterbatch can remove over 40% of the cycle.

The pallet plant data

Metric+15% LLDPE+2% E2625
Cycle time per pallet128 s74 s (−42%)
Daily output, same machine and shift6751167 (+73%)
Daily power usebaseline−1673 kWh (−73%)

The arithmetic

At an industrial tariff of CNY 0.70/kWh, one machine saves 1673 kWh per day:

  • About CNY 1,171 per day in electricity
  • Over 300 days: about CNY 350,000 per year
  • Output up 73% on the same machine also dilutes labour and depreciation

That is usually larger than the annual masterbatch purchase. The correct evaluation puts cycle benefit and additive cost in the same calculation.

Why energy falls 73%

Not all of it is the cycle. Two more effects:

  • Lower melt viscosity (intra-molecular lubrication) reduces screw torque and motor current
  • Lower processing temperature reduces barrel heating power

All three together produce that magnitude. A 42% cycle reduction alone cannot explain a 73% energy reduction — which is why we emphasise that "targeted" means nucleation and lubrication together.

Notes for your trial

  • Do not keep the old process settings. Holding and cooling times can be reduced, otherwise you will not see the benefit
  • Fix other variables and reduce cooling time only, until you reach the shortest time without sink marks or distortion
  • Watch ejection. Faster crystallisation changes shrinkage behaviour; moulds with insufficient draft can show ejector whitening
  • Post-mould shrinkage usually improves, but confirm by measurement

Test it before you price it

Tell us your resin grade, processing temperature, part thickness and the property you need to improve. We recommend a grade and dosage, ship 1–5 kg, and follow up with comparative data.